Dunkin Posted October 12, 2023 Report Share Posted October 12, 2023 What type of plating was used for the hood locks, hood lock bell crank, & rods, hood support, accelerator linkage and the trunk hinges? Thanks. Link to comment Share on other sites More sharing options...
lschuc Posted October 13, 2023 Report Share Posted October 13, 2023 Most of the pieces you mention were cadmium plated. I've found a very good place for CAD plating in the Chicago area. Look up Grove Plating in Fox River Grove, Illinois. They usually charge now about $85 for a bucket of miscellaneous parts. Some larger parts are prices individually. It helps if you can clean all the parts first by bead blasting and cleaning up with a wire wheel. Either ship the bucket or large sturdy box to them, or if you're anywhere in northern Illinois, even within a couple hundred miles, it's usually worthwhile to drive there with your boxes and parts, and let them ship them back to you, one way. Link to comment Share on other sites More sharing options...
Dunkin Posted October 13, 2023 Author Report Share Posted October 13, 2023 Thank you for your information, I live in Texas I will see if anyone can do it locally. Link to comment Share on other sites More sharing options...
ronmanfredi Posted October 16, 2023 Report Share Posted October 16, 2023 You might consider doing a flat silver powder coat also. Link to comment Share on other sites More sharing options...
brad Posted October 24, 2023 Report Share Posted October 24, 2023 On 10/13/2023 at 7:30 AM, lschuc said: Most of the pieces you mention were cadmium plated. I've found a very good place for CAD plating in the Chicago area. Look up Grove Plating in Fox River Grove, Illinois. They usually charge now about $85 for a bucket of miscellaneous parts. Some larger parts are prices individually. It helps if you can clean all the parts first by bead blasting and cleaning up with a wire wheel. Either ship the bucket or large sturdy box to them, or if you're anywhere in northern Illinois, even within a couple hundred miles, it's usually worthwhile to drive there with your boxes and parts, and let them ship them back to you, one way. They do not do CADMIUM plating. What you had done was bright ZINC plating a totally different metal. CADMIUM is no longer legal due to toxicity of the chemicals. Link to comment Share on other sites More sharing options...
Dunkin Posted October 25, 2023 Author Report Share Posted October 25, 2023 Yes, I was thinking that it was banned, I will have to see what I can find down here. Thanks. Link to comment Share on other sites More sharing options...
Recommended Posts
Create an account or sign in to comment
You need to be a member in order to leave a comment
Create an account
Sign up for a new account in our community. It's easy!
Register a new accountSign in
Already have an account? Sign in here.
Sign In Now