mfg Posted June 16, 2019 Report Share Posted June 16, 2019 Studebaker Service letter W-1963-1 dealt with the use of acrylic lacquer paint. (which was originally used on Studebaker Avantis) The most common post-production paint defect reported to the factory was......?...... 1) 'Shadowing'.....2) Blisters.....3) Cracking.....or.....4) Poor Adhesion Link to comment Share on other sites More sharing options...
studegary Posted June 16, 2019 Report Share Posted June 16, 2019 4 hours ago, mfg said: Studebaker Service letter W-1963-1 dealt with the use of acrylic lacquer paint. (which was originally used on Studebaker Avantis) The most common post-production paint defect reported to the factory was......?...... 1) 'Shadowing'.....2) Blisters.....3) Cracking.....or.....4) Poor Adhesion 2) blisters - "...the formation of small blisters under the surface of the paint." Link to comment Share on other sites More sharing options...
mfg Posted June 16, 2019 Author Report Share Posted June 16, 2019 1 hour ago, studegary said: 2) blisters - "...the formation of small blisters under the surface of the paint." And you are CORRECT! Link to comment Share on other sites More sharing options...
Recommended Posts
Create an account or sign in to comment
You need to be a member in order to leave a comment
Create an account
Sign up for a new account in our community. It's easy!
Register a new accountSign in
Already have an account? Sign in here.
Sign In Now